transparent glass turns opaque

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

transparent glass turns opaque

Post by Michael Stevens »

I fused some red glass and it was fine, but I. used similar glass and did a lot melt at higher than fusing temps and it turned opaque, the other colors were fine, I thought maybe debit but it's happened 2 times same color.

does this happen to anyone
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: transparent glass turns opaque

Post by Brad Walker »

Very common, especial with reds. The higher the temperature, the more likely.
Post Reply