I made some molds from shells as casted them, they have nice texture if I tack fuse to a project will the texture be flattened. Or is the only solution to glue. them on?
I guess I could use powdered glass and paint the details to look like the pattern. but I was hoping to. keep the original pattern, my daughter collected. these shells so I wanted a special piece.
keeping Texture on glass
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: keeping Texture on glass
If you tack fuse at a low enough temperature you'll keep most of the texture. 1350F/730C is high enough to stick glass together and retain most of the texture. The higher above that you go, the more texture you will lose.
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: keeping Texture on glass
Use a low temperature flux, or a glass paint as a glue. I've done a lot of these.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns