can't figure out what I. did different

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

can't figure out what I. did different

Post by Michael Stevens »

I added mica powder and it created beautiful blue bubble, but now I'm getting dark black lines and some spots of gold in. the center. I'm. not sure if I changed heating schedule, mixed different portion of powder and glycol, I'm. trying to duplicate result but can't understand why things are different
IMG_20200424_202709.jpg
IMG_20200424_201652.jpg
IMG_20200424_201443.jpg
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: can't figure out what I. did different

Post by Brad Walker »

You sure it's mica powder you added? Looks like copper or a copper oxide.
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: can't figure out what I. did different

Post by Michael Stevens »

maybe it has additives but it's gold mica powder. did I not fire hot or long enough, is that why center stayed gold color? or the black lines is that from contamination with other powders?
IMG_20200425_230012.jpg
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: can't figure out what I. did different

Post by Brad Walker »

Generally, blue bubbles come from a copper compound. They'll give you the beautiful bright blue bubbles in your piece. If you put too much copper (usually copper oxide) it will have black ugly areas like your other piece. Firing too high can also cause this problem.

My guess is that the mica you're using has come copper oxide in it. Try using less of the mica and see if you get a better result.
Post Reply