Post by Heapsy »

Hi,
Can I use the ceramic gold luster for fused glass?
I did use it but it has like stain and puddles on the glass.
I fired to 1300F or do I need to fire higher? Thanks
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Ceramic gold luster

Post by Barry Kaiser »

Works fine on glass
Needs to be applied very thin, not puddling.
Vent the kiln up to 1000 then close.
Works well but is difficult to apply.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Ceramic gold luster

Post by Barry Kaiser »

Forgot:
Two types, but you probably have the one that fully matures at about 1350 (but 1300 usually works fine)
Other kind matures lower.
Heapsy
Posts: 7
Joined: Thu May 22, 2014 10:11 am

Re: Ceramic gold luster

Post by Heapsy »

Thank you.
Works fine on glass
Needs to be applied very thin, not puddling.
Vent the kiln up to 1000 then close.
I do all of that but still not good, maybe it's that band I'm using, I didn't had these problems on the glass but this one is the first time I purchased from pottery Supply before I had one been given to me and was fine, and before that I purchased from fused glass supplies
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Ceramic gold luster

Post by Barry Kaiser »

What is the brand.
Delarobbia and Duncan are the most common ones.
Heapsy
Posts: 7
Joined: Thu May 22, 2014 10:11 am

Re: Ceramic gold luster

Post by Heapsy »

What is the brand.
I don't know, it doesn't say on the bottle, I bought it from the pottery Supply
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Ceramic gold luster

Post by Barry Kaiser »

That is quite unusual. The stuff is quite precious and usually is sold in a small (2dram) sealed bottle.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Ceramic gold luster

Post by Brad Walker »

I suspect you two are talking about two different products. The term "luster" is often used to refer to anything that's shimmery. For example, Thompson uses the word "luster" to refer to their micas.

Heapsy, to you have a link to the pottery supplier that sold you the product? Or is there more information on the label than just the name?
Heapsy
Posts: 7
Joined: Thu May 22, 2014 10:11 am

Re: Ceramic gold luster

Post by Heapsy »

Its about real liquid gold.
They don't have a link.
But I just got reply I asked about what temperature to fire, so he said 720 Celsius (1328F) and I fired it to 704 Celsius (1299F) so maybe that is the reason