I would like[fimg=][/fimg] to know how to create nice crisp lines between different colored powders and fine frit
like this pic
The other Jim
crisp lines with powders and frit
Moderators: Brad Walker, Tony Smith
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: crisp lines with powders and frit
when I sift or brush on powders and frit, I create barriers using bendable plastic ruler. stencils or brush.
or could use a stringer bent to shape then glued down if you want border line. and fill in. like cloisone style
or could use a stringer bent to shape then glued down if you want border line. and fill in. like cloisone style
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: crisp lines with powders and frit
You could use Liquid Glassline and then fill in with frit. Google it - Richard La Londe. Basically CMC & glass powder, piped through a cake decorating bag. There's a free tutorial out on the internet somewhere.
Dana W.
Dana W.
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: crisp lines with powders and frit
Thanks, Dana.
The other Jim
The other Jim