Multiple high hest firings

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Multiple high hest firings

Post by Doug Zawodny »

Does anyone know if firing multiple times (5-7) at 1600 and higher makes the glass unstable?
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Multiple high temperature firings

Post by Brad Walker »

It does.

I'd be leery of firing more than once (and twice at the most) at temperatures above 1600F/870C. Incompatibility can result. It's especially likely with whites, with glasses containing aventurine, with glasses containing gold, and with pieces you absolutely don't want it to happen.
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Re: Multiple high hest firings

Post by Doug Zawodny »

Thanks Brad. That explains my problem.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Multiple high hest firings

Post by Kevin Midgley »

When Bullseye first started there were some colours that you could fuse but try a second firing and it would break.
Now the description I believe is 3 full fuse firings.
Since fuse firings are nowhere near those temperatures you are way over any chances of stability.
I only fire glass twice for that reason.