Schedule for kiln pressed glass - for Uroboros

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Schedule for kiln pressed glass - for Uroboros

Post by Havi »

Hello everybody,
I discovered a nice pack of Uroboros glass in my storage.
Some of it is very nice colors.Eventhough its COE is 90 - it is fired on different schedule than BE.

Being weak in numbers, I would appreciate it if anybody could refer me to Uroboros firing schedule for SMOOSHED GLASS, or UNDER PRESSURE or KILN PRESSED GLASS - those are all names of the same process.

I'd be more than grateful!!!


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Post by Brad Walker »

I never fired Uro 90 that much (if any) different than Bullseye. The same schedule ought to work.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Post by Havi »

Thank, Brad

My best teacher!

Did you also mix BE AND URO????

many thanks in advance

H
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Post by Brad Walker »

Havi wrote:Did you also mix BE AND URO????
Always the clear Uro with BE, no problems. Sometimes the other colors. Only problem I ever experienced was with one of the Uroboros reds. Not surprising since reds can be difficult to make.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Post by Havi »

Thanks a lot, Brad

Always appreciate your knowledge,
and
your
sharing it!!!

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Post Reply