Schedule for slumping large piece, 9mm thick?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Schedule for slumping large piece, 9mm thick?

Post by Nina Falk »

Suggestions for a schedule to safely slump a 9mm piece, 34" x 20"? Slumping over a stainless steel mold, using 1/16" fiberboard.
Thinking of
75 1150 60
Full 930 ??

Thanks!
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Schedule for slumping large piece, 9mm thick?

Post by Brad Walker »

That schedule would probably work. For over stainless I usually watch the piece and just hold until it's done the way you want it, however long that takes. 75 on the way up is conservative, but justifiable on a piece that large. I assume you're not really close to the top elements.

Bullseye would say to anneal at 900 but 930 works, too. Hold two hours or more to be safe.

Big piece!
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: Schedule for slumping large piece, 9mm thick?

Post by Nina Falk »

Thanks so much, Brad! Yes, it's big...going in my backyard.
Susie sargent
Posts: 4
Joined: Mon Jan 19, 2004 5:07 am
Location: Berkeley, CA

Re: Schedule for slumping large piece, 9mm thick?

Post by Susie sargent »

Nina, further to Brad's reply, I think you will find Bullseye's annealing schedule PDF helpful in the future. If you Google "bullseye glass annealing schedule" you will find the PDF.
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: Schedule for slumping large piece, 9mm thick?

Post by Nina Falk »

it's all slumped, turned out beautifully!