Suggestions for a schedule to safely slump a 9mm piece, 34" x 20"? Slumping over a stainless steel mold, using 1/16" fiberboard.
Thinking of
75 1150 60
Full 930 ??
Thanks!
Schedule for slumping large piece, 9mm thick?
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Schedule for slumping large piece, 9mm thick?
That schedule would probably work. For over stainless I usually watch the piece and just hold until it's done the way you want it, however long that takes. 75 on the way up is conservative, but justifiable on a piece that large. I assume you're not really close to the top elements.
Bullseye would say to anneal at 900 but 930 works, too. Hold two hours or more to be safe.
Big piece!
Bullseye would say to anneal at 900 but 930 works, too. Hold two hours or more to be safe.
Big piece!
Re: Schedule for slumping large piece, 9mm thick?
Thanks so much, Brad! Yes, it's big...going in my backyard.
-
Susie sargent
- Posts: 4
- Joined: Mon Jan 19, 2004 5:07 am
- Location: Berkeley, CA
Re: Schedule for slumping large piece, 9mm thick?
Nina, further to Brad's reply, I think you will find Bullseye's annealing schedule PDF helpful in the future. If you Google "bullseye glass annealing schedule" you will find the PDF.
Re: Schedule for slumping large piece, 9mm thick?
it's all slumped, turned out beautifully!