Post by jim burchett »

I have made pieces in the past with Silver foil on BE reactive Ice and gotten a nice fume pattern. I am wondering if I use Tekta and Reactive Ice powder with Silver it will give a similar effect?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Silver Fuming

Post by Brad Walker »

Silver needs to be on top for best results, but would work.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Silver Fuming

Post by jim burchett »

Thanks, I always put the silver on top, I will run a cpl of text tiles tonight.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Silver Fuming

Post by Brad Walker »

jim burchett wrote:text tiles
Test me the results. :D
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Silver Fuming

Post by jim burchett »

While it did react, and there was some Halo, it wasn't nearly as intense as on the glass itself. Tried several different thicknesses of the powder, but it distorted the transparency in relation to its depth. So, these will just cost more in the future. So the answer is Yes, but....
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Silver Fuming

Post by jim simmons »

Maybe try to fuse the powder first then refuse with the silver?
The oher Jim
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Silver Fuming

Post by jim burchett »

Too many steps then