Adhesives for securing frit and little glass components
Moderator: Tony Smith
Adhesives for securing frit and little glass components
I know people use a variety of adhesives when piling up powder, frit and cut-ups on a flat blank. Why do you do this? Is it to keep the stuff from moving while you pile it up, or when you move it to the kiln? Or does it actually add some stability during the firing process? I haven’t used glue to hold stuff. I figured it would exacerbate movement as it burns out in the kiln. But I’m not certain. If you would share you thoughts I would appreciate it.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Adhesives for securing frit and little glass components
just used to keep the frit from moving when the kiln shelf is moved.
The other Jim
The other Jim
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Adhesives for securing frit and little glass components
burns off around 300F ..don't expect it to hold stuff in place for fusing