Slumping a double curve mould

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
annieontherun
Posts: 1
Joined: Sun Mar 06, 2022 9:12 am

Slumping a double curve mould

Post by annieontherun »

Hi you bunch of geniuses!

I'm just about to slump a piece of bullseye glass which is 3mm thick 10" x 6" and has been fused with frit powders. How long should the ramp time be and to what temperature? Sorry to ask such an obvious question but I am mystified & very nervous as its my first ever attempt in my kiln which is a Hobbyfuser 4 if thats any help?!
Thanks in advance my brain hurts!!

Annie
Brad Walker
Site Admin
Posts: 1536
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Slumping a double curve mould

Post by Brad Walker »

Bullseye has recommended schedules on their website for all of their molds: http://www.bullseyeglass.com/methods-id ... dules.html

For non-Bullseye molds, just find a similar shape on their recommended list.
Post Reply