Polishing Question
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Polishing Question
Hi, I am trying to get a clear polish on all sides with a Somaca wet belt sander, I am wondering if I can use cerium oxide with my Cork belt? Can't seem to find a 4x106 felt belt. THANKS
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Polishing Question
You can polish with just a cork belt. No need to use cerium oxide, but cork does like more water than other belts.
Re: Polishing Question
I used to use cork but they wear easily. Now I use a trizact 1800 belt, then felt with pumice and end with a felt and cerium. all available at HISglassworks