Polishing Question

Post by jim burchett »

Hi, I am trying to get a clear polish on all sides with a Somaca wet belt sander, I am wondering if I can use cerium oxide with my Cork belt? Can't seem to find a 4x106 felt belt. THANKS
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Polishing Question

Post by Brad Walker »

You can polish with just a cork belt. No need to use cerium oxide, but cork does like more water than other belts.
Dick
Posts: 89
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Polishing Question

Post by Dick »

I used to use cork but they wear easily. Now I use a trizact 1800 belt, then felt with pumice and end with a felt and cerium. all available at HISglassworks