Post by Karen L »

Hello
I have been given some Hotline glass stringers with a catalog number 4955, 4954 and Millefiori slices number 1554. Can anyone help with the COE of these?

Thanks

Karen Layton
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Hotline Glass

Post by AndyT »

Karen L wrote:Hello
I have been given some Hotline glass stringers with a catalog number 4955, 4954 and Millefiori slices number 1554. Can anyone help with the COE of these?

Thanks

Karen Layton
The Mille is 104. The stringers could be 90 or 96. Hotline products are from Creative Craftsman. https://gofusing.com/brands/Hotline-by- ... -Inc..html