Modifying a slumping mold

Post by makeart365@gmail.com »

I have a large (20”) ball mold I would like to make undulate on the side surface. It would only need a few areas bumped in to make it more organic. Can this be done with fiber paper or ???
Thanks, Linda
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Modifying a slumping mold

Post by Brad Walker »

Fiber paper will work.
makeart365@gmail.com
Posts: 3
Joined: Sat Oct 31, 2020 9:39 pm

Re: Modifying a slumping mold

Post by makeart365@gmail.com »

Fiber paper is so thin I don’t know how I would get any raised fluted shape. Is there something to build up the surface under the fiber paper?
Thanks!
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Modifying a slumping mold

Post by Brad Walker »

Fiber paper comes in thicknesses from 1/32" to 1/4". You may be thinking of thinfire paper, which is much thinner.

You could also use fiber blanket, which comes in thicknesses from 1/2" to 4".
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Modifying a slumping mold

Post by JestersBaubles »

These were made in 5" ball surface molds. I used SilkMatte. It works fine for larger pieces as well.
DSCN3659edited-small.jpg
Best, Dana