Hi everybody,
Long time no see,
good to be back here, and good to see some familiar names.
This board had always helped me [I mean to people who participate..] Hope you are all well!
I want to polish a piece by covering it with BE cloear transparent powder [1401 or 1101 /08] what temprature should I reach?
I apologise for having forgotten this basic , and of course I shall check the kiln while firing to the top temp.
I have zillions of notes, so I prefer asking someone who knows this off his sleeve..
Many thanks in advance,
Havi
Polishing by using Glass powder - at what temp.?
Moderators: Brad Walker, Tony Smith
Polishing by using Glass powder - at what temp.?
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Polishing by using Glass powder - at what temp.?
I fire to around 1440F/780C with a 5 to 10 minute hold.
Re: Polishing by using Glass powder - at what temp.?
Thanks Brad,
Hopefully will fire tonight
Havi
Hopefully will fire tonight
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Polishing by using Glass powder - at what temp.?
Hi Havi, will we see a photo??
Re: Polishing by using Glass powder - at what temp.?
Hopefully there will be what to show
Then, I'll post a photo
Thanks for the interest.
H.
Then, I'll post a photo
Thanks for the interest.
H.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Polishing by using Glass powder - at what temp.?
Hi everybody,
As promised, I shall try post the results. To be honest the peice went thru several additional firings, as it did not shine enough. Then i added the stringers, and realized it was too much, so, refired and covered part................
Once I saw the piece, its name hit me HEAT WAVE
.attachment=0]גל חום 2.jpg[/attachment]
As promised, I shall try post the results. To be honest the peice went thru several additional firings, as it did not shine enough. Then i added the stringers, and realized it was too much, so, refired and covered part................
Once I saw the piece, its name hit me HEAT WAVE
.attachment=0]גל חום 2.jpg[/attachment]
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com