Drop out

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Drop out

Post by Doug Zawodny »

Long story short. I have a piece that only dropped 3 of the 7in. My question is, can I start a new drop schedule with the glass being different thicknesses without it cracking?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Drop out

Post by Kevin Midgley »

Heat it up super slowly and you should be fine.
Post Reply