Slump breakage
Moderators: Brad Walker, Tony Smith
-
makeart365@gmail.com
- Posts: 3
- Joined: Sat Oct 31, 2020 9:39 pm
Slump breakage
All spectrum (96coe) used. Same schedule as used before and other pieces in kiln were fine. When lifted out of mold end pieces broke. Don’t think it is incompatibility since all labeled 96. What else could it be?
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Slump breakage
Schedule?
Were other pieces the same? i.e. same mold?
Were other pieces the same? i.e. same mold?