Slump breakage

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
makeart365@gmail.com
Posts: 3
Joined: Sat Oct 31, 2020 9:39 pm

Slump breakage

Post by makeart365@gmail.com »

All spectrum (96coe) used. Same schedule as used before and other pieces in kiln were fine. When lifted out of mold end pieces broke. Don’t think it is incompatibility since all labeled 96. What else could it be?
IMG_5679.jpeg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Slump breakage

Post by Brad Walker »

Schedule?

Were other pieces the same? i.e. same mold?
Post Reply