Piece cracked on slump

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Piece cracked on slump

Post by jim burchett »

Third slump of a Deep Bowl and this happened.how to prevent this In future?
16997217735336917883643605956463.jpg
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Piece cracked on slump

Post by Brad Walker »

Schedule? Mold?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Piece cracked on slump

Post by Kevin Midgley »

Less heatwork, slower heating and longer annealing. Bullseye says three firings. Based on my experience with the early formulations of Bullseye where the COE could shift, my policy is to do no more than 2 firings. That requires rethinking what shapes you make, the molds you use and firing schedules. I can easily fire in a single long firing a 4 layer bowl that everyone else takes multiple firings to complete. That pattern you have could have been done in one firing.