Hi everybody,

How would I dam a circle about 12" to 15" round, NOT having SS in Israel...

I would appreciate your comments.

many thanks,
Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: damming circles

Post by Brad Walker »

Wrap fiber paper around the circle. Two times around is best. Then hold it in place with LOTS of kiln posts.
Attachments
BirdBath.jpg
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: damming circles

Post by Havi »

Thanks, dear Brad!

Can I use additionally copper sheet to strengthen the fiber? [not sure I have that many kiln posts]


Thanks
Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: damming circles

Post by Brad Walker »

I'm not sure I'd use copper, not that strong. But you could confine the paper with nichrome (high temperature) wire instead of the posts.

Instead of posts, you could use cut up kiln shelves or kiln bricks (though the latter isn't as heavy as you'd prefer).
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: damming circles

Post by Havi »

Many thanks, Brad

However, I forgot the most important issue -
I plan to create a round sheet from scrap - and this is more problematic, I am afraid.
I want to do a piece with powders - the way Parrish works, -
Hope to be successful

thanks again,
Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: damming circles

Post by Brad Walker »

Yes, scrap is more problematic. I would consider having a clear circle of glass as the base and build on top of that.
danieljanse
Posts: 9
Joined: Sat Feb 02, 2019 5:37 pm

Re: damming circles

Post by danieljanse »

I tried doing this but the paper did not want to stand on it's own. Does this work with Bullseye thin shelf or are you using a thicker variety?
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: damming circles

Post by Havi »

Hi
I am busy with other stuff, have not yet reached this..
Once I get there I shall post my thoughts and performance. I think i shall use 3m'm fiber paper.

Thanks,

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: damming circles

Post by Brad Walker »

danieljanse wrote: Sat Dec 30, 2023 2:30 pm I tried doing this but the paper did not want to stand on it's own. Does this work with Bullseye thin shelf or are you using a thicker variety?
Thinfire doesn't work standing up. You have to use regular fiber paper, 3mm or thicker.
danieljanse
Posts: 9
Joined: Sat Feb 02, 2019 5:37 pm

Re: damming circles

Post by danieljanse »

Thanks, Brad. I'm realizing I need to have a supply of both in the studio. The extra thickness also helps keep the glass and ring from getting too intimate.