A consistent layer of powder frit?
Moderators: Brad Walker, Tony Smith
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
A consistent layer of powder frit?
I need to overlay some imagery on glass with a layer of clear powder frit. I need to achieve a thin layer that is consistent in thickness across the entire piece and that is repeatable on other pieces. I am contemplating dry screening the powder with a 110 mesh screen but I thought that I would see if anyone has any other ideas of how to do this.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: A consistent layer of powder frit?
A dry screen print is probably the easiest way.
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: A consistent layer of powder frit?
Thanks Brad. I just thought that I would see if anybody had any other possibilities.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: A consistent layer of powder frit?
The only other option I can think of is to sift by hand. I'm not capable of doing that evenly enough, but my wife is.
If you were laying down a thick layer you could use a screed (like a straightedge) to even it out, but that won't work for a thin layer.
If you were laying down a thick layer you could use a screed (like a straightedge) to even it out, but that won't work for a thin layer.
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: A consistent layer of powder frit?
Yeah, I have tried hand sifting but even with larger sifters it isn't even enough. I will try the screen technique and hopefully it will do the job.
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: A consistent layer of powder frit?
I just thought that I would mention that the powder screening worked well to get the even layer that I needed. I did learn though that you need either a new screen or one that is perfectly clean for consistency. The first screen that I used had a little haze in it left over from wet media screening and it left an uneven deposit of frit.