Does anyone know if glass becomes less stable the more times it’s fired to 1600?
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Used glass
It will.