Has anyone used Amaco glass? I found several sample boxes, its all marked COE 90. I use 96. I've done a few firings with the Amaco using a schedule that works for 96 (not mixing the 90 and 96) and so far so good. I suspect this stuff is old.
IMG_6077.jpg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Amaco Glass

Post by Brad Walker »

You're right, it's really old stuff, 10 to 15 years old.

For a short period back then Amaco had a fusible line, but it didn't last long. Not sure if it was made by Bullseye or someone else, but it's 90COE, just don't mix it with your 96.