rescue magnetic backing flat lap disc

Post by Marian »

The magnetic backing on my 24 inch diamond disc is coming off. Any advice to re attach? Separately, I got a new disc with no backing at all, just steel. Any way to put a magnetic sheet on that? Did I learn my lesson to read the description more carefully? I'm thinking of attempting contact adhesive and a roll of magnetic sign material as I can't return it.
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: rescue magnetic backing flat lap disc

Post by Marty »

That's exactly what you do- contact cement for the separation and new mag for the other.
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: rescue magnetic backing flat lap disc

Post by Marian »

Thanks! Ok, ordered the magnet sheet.