Can I use hot glue in my kiln?
Moderators: Brad Walker, Tony Smith
-
Linda Jean
- Posts: 3
- Joined: Sat Nov 09, 2024 5:01 pm
Can I use hot glue in my kiln?
I’m making some Christmas decorations with my grandchildren and we have glued glass strips together to make stars with hot glue. They aren’t great works of art so I’m not too concerned how they will look, just want them to hold together to get them into the kiln. My concern was that the glue residue may harm the elements on the kiln in some way. Just wanted to check before I fire them. Thought?
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Can I use hot glue in my kiln?
Yes, you can use hot glue, just don't overdo it.
-
Linda Jean
- Posts: 3
- Joined: Sat Nov 09, 2024 5:01 pm
Re: Can I use hot glue in my kiln?
Thanks Brad, what’s going to happen if you overdo it? Just concerned about the residue harming the kiln. Thanks. 
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Can I use hot glue in my kiln?
There won't be any harm to the kiln. The worst thing that can happen is that you get little black carbon spots on the glass.
-
Linda Jean
- Posts: 3
- Joined: Sat Nov 09, 2024 5:01 pm
Re: Can I use hot glue in my kiln?
Thanks so much. Will see how it goes!