No Days glass fusing glue

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

No Days glass fusing glue

Post by Terry Gallentine »

Does anyone have any experience with No Days glass fusing glue? I need a glue that is not water soluble like Glastac is and I have read that No Days is not water soluble. Are there other alternatives to Glastac that are not water soluble and not the older suggestions such as super glue?
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: No Days glass fusing glue

Post by Brad Walker »

You might ask the No Days people: https://nodaysadhesives.com/No-Days-Liq ... g-c5749935

Don't know if it will work for you, but hot glue is polymer based so shouldn't be water soluble. It burns off pretty clean, but you may want to test for your application if you try it.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: No Days glass fusing glue

Post by Terry Gallentine »

Thanks Brad.
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: No Days glass fusing glue

Post by Vonon »

I've used hot glue without a problem.
Vonon
Post Reply