No Days glass fusing glue
Moderators: Brad Walker, Tony Smith
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
No Days glass fusing glue
Does anyone have any experience with No Days glass fusing glue? I need a glue that is not water soluble like Glastac is and I have read that No Days is not water soluble. Are there other alternatives to Glastac that are not water soluble and not the older suggestions such as super glue?
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: No Days glass fusing glue
You might ask the No Days people: https://nodaysadhesives.com/No-Days-Liq ... g-c5749935
Don't know if it will work for you, but hot glue is polymer based so shouldn't be water soluble. It burns off pretty clean, but you may want to test for your application if you try it.
Don't know if it will work for you, but hot glue is polymer based so shouldn't be water soluble. It burns off pretty clean, but you may want to test for your application if you try it.
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: No Days glass fusing glue
Thanks Brad.