slump after sandblast?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

slump after sandblast?

Post by Bonnie Rubinstein »

Hi All, I may have made a mistake, I applied all the resist areas to glass that I will sandblast, but it slipped my mind (how?) that I planned to slump them. Can I blast and then slump (easy slump into platter mold), or do I risk diminishing the blasted texture? The slump will be at about 1250. thanks.
Bonnie Rubinstein
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: slump after sandblast?

Post by Brad Walker »

At 1250F most of the sandblasted surface will start to shine.

If you can, go to around 1125 and hold for an hour. That works for most shallow molds and will leave you a very nice matte surface. (My favorite finish, by the way.)
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: slump after sandblast?

Post by Bonnie Rubinstein »

so, if I want it to be stronger texture than a matte finish, this will not work?
Bonnie Rubinstein
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: slump after sandblast?

Post by Brad Walker »

I guess it depends on how low you can go and still achieve the slump you want. The lower the better, the shorter hold the better.

You could test with a scrap to see if you like the resulting texture.
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: slump after sandblast?

Post by Bonnie Rubinstein »

Good suggestion, Brad. Thank you.
Bonnie Rubinstein