I have several partial sheets of Blenko glass plus many formed pieces that were discarded due to breakage. I've done compatibility testing with Bullseye and made a chart of "no goes". I want to break up some of the chunky stuff and fire it flat. I know it should be slow but is there a too slow? The fellow that let me climb into the dumpster said I could treat it like 90 coe. Any suggestions?
Vonon
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Blenko Glass
I wouldn't assume it's 90 COE, so good thing you're testing.
It may devitrify.
Too slow not really an issue.
It may devitrify.
Too slow not really an issue.
Re: Blenko Glass
Thank you Brad. Of the colors I tested with Bullseye, only the red developed incompatibility cracks
. I actually haden't thought about devit. Maybe I'll just donate it to a local stained glass artist.