Post by Vonon »

I have several partial sheets of Blenko glass plus many formed pieces that were discarded due to breakage. I've done compatibility testing with Bullseye and made a chart of "no goes". I want to break up some of the chunky stuff and fire it flat. I know it should be slow but is there a too slow? The fellow that let me climb into the dumpster said I could treat it like 90 coe. Any suggestions?
Vonon
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Blenko Glass

Post by Brad Walker »

I wouldn't assume it's 90 COE, so good thing you're testing.

It may devitrify.

Too slow not really an issue.
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Blenko Glass

Post by Vonon »

Thank you Brad. Of the colors I tested with Bullseye, only the red developed incompatibility cracks :( . I actually haden't thought about devit. Maybe I'll just donate it to a local stained glass artist.
Vonon
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Blenko Glass

Post by Brad Walker »

Vonon wrote: Mon May 25, 2026 2:22 pm Of the colors I tested with Bullseye, only the red developed incompatibility cracks
Red's almost always incompatible, no matter who made it.