I'm wanting to add a different thermocouple to my kiln and I need some of the ceramic tubing that the TC wire is passed thru, into the kiln.
Does anybody know of a reasonable source for these ??  Ideally, I'd like 4 hole, as I might add a seperate TC for an overtemp alarm.
I've seen them made of mullite and alumina.  Need the 1/4" OD size.
I'd probably like to get several, to have some spares for the future.
Bill
			
			
									
						
							Ceramic 2/4 hole tubing
Moderators: Brad Walker, Tony Smith
Ceramic 2/4 hole tubing
Visit my Art Glass Answers forum
[url]http://www.artglassanswers.com/forum
			
						[url]http://www.artglassanswers.com/forum
- 
				Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
I think this is what you want: http://www.sisweb.com/ms/sis/certb-4.htm
Google search on "thermocouple insulator" and you'll get a lot of different sites with similar products.
			
			
									
						
										