( Norton h20 proof 120 grit sand paper available at homedepot)
Norton drywall screen for removal of kiln wash
Moderators: Brad Walker, Tony Smith
-
Kelly & Charlie MacMu
Norton drywall screen for removal of kiln wash
Thanks AVLucky!! It took probably less than 2 minutes to clean off 3 kiln shelves. I had a respirator on ( lots of dust ) great Idea
The stuff cost about $10.00 for ten sheets of it.
( Norton h20 proof 120 grit sand paper available at homedepot)
( Norton h20 proof 120 grit sand paper available at homedepot)