I am about to cast some lotus flowers with Gaffer 300 Opaline. I have billets. Am I only going to get an opal white out of it? Anyone with experience with this stuff? Here are some links from ocr:
http://www.glasscolor.com/catalog/color ... ting%2Easp
http://www.glasscolor.com/conferencecal ... uestion=83
Thanks!
Gaffer 300 Opaline: Have I shot myself in the foot?
Moderator: Brad Walker
-
jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
Gaffer 300 Opaline: Have I shot myself in the foot?
j.
A lack of doubt doesn't lend certainty.
A lack of doubt doesn't lend certainty.
-
charlie holden
- Posts: 260
- Joined: Thu Mar 13, 2003 8:26 pm
- Location: Atlanta
-
jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
Yeah, Charlie, that's what I read too. I was wondering if anyone had experienced it though... Client purchased color. The whole pallet of choices and, of course, she picks the hardest color.
I am thinking about maybe bringing the billets to 1000 (in a porcelain cup) and then slamming them in a glory hole. I think the whiteness is that the billets have been annealled and had more time to build up crystal structure. So even though the billets are clear they are more mature than the frit. Maybe if I can jack them up from 1000 to 1400-1500 in like three or four minutes and then pour them into a hot mold Maybe I can cut down on the amount of time they would get to strike in a natural kiln kasting scenario... Maybe.
Maybe someone else has cast with these billets and has some notes?
I am thinking about maybe bringing the billets to 1000 (in a porcelain cup) and then slamming them in a glory hole. I think the whiteness is that the billets have been annealled and had more time to build up crystal structure. So even though the billets are clear they are more mature than the frit. Maybe if I can jack them up from 1000 to 1400-1500 in like three or four minutes and then pour them into a hot mold Maybe I can cut down on the amount of time they would get to strike in a natural kiln kasting scenario... Maybe.
Maybe someone else has cast with these billets and has some notes?
j.
A lack of doubt doesn't lend certainty.
A lack of doubt doesn't lend certainty.