Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable
Thanks Randy
Thanks Randy
Re: Mother of Pearl Powders
Compatability won't be a problem, but what is this stuff? If it's real nacre, it's just gonna burn up. Maybe they're another form of mica? Brocknbaybear wrote:Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable