Bullseye sample sets- Striking Colors
Moderators: Brad Walker, Tony Smith
- 
				Steve Immerman
- Posts: 208
- Joined: Sun Mar 09, 2003 4:55 pm
- Location: Eau Claire, Wisconsin
- Contact:
Bullseye sample sets- Striking Colors
I have one of Bullseye's Kilnforming Sample sets, that I've had for about 8 years now, and have added updates a couple of times. I just ordered the 2003 update so I could see exactly what some of the new, cool, colors look like.
To my disappointment, all the striking colors came "unstruck" with a label that says someting to the effect "Strikes to Sunset Coral upon firing"
Am I missing something here, or does that make those samples kind of useless for kilnformers?
I suppose I could fire the samples, or buy sheets and make my own reference samples - but that sort of obviates the value of buying a sample set. I use these as color references when ordering glass. So, how am I going to compare, for example, the "violet striker" to light plum, light violet neo lavender etc when I can't see the color.
Is the issue that it strikes to different colors depending on the fusing temp?
I just found this kind of odd. I think it would be nice if they included both the struck and unstruck color. Or an extra piece so we can create our own striking sample.
Yes, I know I'm ranting. Sorry.
Steve
			
			
									
						
										
						To my disappointment, all the striking colors came "unstruck" with a label that says someting to the effect "Strikes to Sunset Coral upon firing"
Am I missing something here, or does that make those samples kind of useless for kilnformers?
I suppose I could fire the samples, or buy sheets and make my own reference samples - but that sort of obviates the value of buying a sample set. I use these as color references when ordering glass. So, how am I going to compare, for example, the "violet striker" to light plum, light violet neo lavender etc when I can't see the color.
Is the issue that it strikes to different colors depending on the fusing temp?
I just found this kind of odd. I think it would be nice if they included both the struck and unstruck color. Or an extra piece so we can create our own striking sample.
Yes, I know I'm ranting. Sorry.
Steve
Striking color
I just ordered from BE and it does show the before and after strike color in their new catalog. Unfortunately you are correct, yes you will need to fire the glass at fuse temp to get the strike color.  I also WAS going to order some of them, but like you I did not want to keep samples of the strike color after fuse, after all these little buggers begin to creep into my space more than I like. Hope that helped, good luck.
camaro
			
			
									
						
										
						camaro
- 
				The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Doc, you're behaving too scientifically....stop it!
Of course it would make sense to send them "struck", in fact it would be even more sensible to send two pieces, before and after since that is the nature and selling(?) point of the glass.
Just go fire them and then order another set so you'll have both. You're forgiven for ranting.
Jim
			
			
									
						
							Of course it would make sense to send them "struck", in fact it would be even more sensible to send two pieces, before and after since that is the nature and selling(?) point of the glass.
Just go fire them and then order another set so you'll have both. You're forgiven for ranting.
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
			
						- 
				Barbara Cashman
- Posts: 151
- Joined: Sun Mar 09, 2003 5:42 pm
- Location: Greensboro NC
- Contact:
I just placed an order directly with BE because I couldn't find their new Opal Olive Green with any of my other suppliers. I mentioned that I wished BE made a "caramel" brown and Taylor said they do. It's just one of their special order colors.   
 
Special order colors !!! "Ooohhh, I asked, what else is available in special order?" Well, they have, in addition to the caramel, a Persimmon Red, Spicy Orange (hoping this is a terra cotta color), Tomato Red and deep red. I've ordered 10x10 of each of those, but they don't have ANY larger sheets of the Olive](./images/smilies/eusa_wall.gif) which was the reason for the call.  They don't sell samples of their special colors. Smallest size is 10x10.
 which was the reason for the call.  They don't sell samples of their special colors. Smallest size is 10x10.
Steve, I only have BE stained glass sample sets. I'm glad you posted because I've often though I was missing out because I didn't have the kiln forming set. I assumed, like you, that they'd send fired samples. No logic in Corporate America.
I fire small (5mm) square samples of all my glass. I keep it in a white dish in the shop. It's helped me alot when picking colors.
Just my .02 ...Kelly
			
			
									
						
										
						 
 Special order colors !!! "Ooohhh, I asked, what else is available in special order?" Well, they have, in addition to the caramel, a Persimmon Red, Spicy Orange (hoping this is a terra cotta color), Tomato Red and deep red. I've ordered 10x10 of each of those, but they don't have ANY larger sheets of the Olive
](./images/smilies/eusa_wall.gif) which was the reason for the call.  They don't sell samples of their special colors. Smallest size is 10x10.
 which was the reason for the call.  They don't sell samples of their special colors. Smallest size is 10x10.Steve, I only have BE stained glass sample sets. I'm glad you posted because I've often though I was missing out because I didn't have the kiln forming set. I assumed, like you, that they'd send fired samples. No logic in Corporate America.
I fire small (5mm) square samples of all my glass. I keep it in a white dish in the shop. It's helped me alot when picking colors.
Just my .02 ...Kelly
- 
				Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
They have lots of special colors that aren't considered stock. But they only have them sometimes, so don't get spoiled with one! Spicy Orange is not really Terra Cotta colored. I happen to love the color, so if you know my pallette, that should give you some idea of what it's like. Tomato too. Yum!Special order colors !!! "Ooohhh, I asked, what else is available in special order?" Well, they have, in addition to the caramel, a Persimmon Red, Spicy Orange (hoping this is a terra cotta color), Tomato Red and deep red.
- 
				Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
Yeah, that bugged me too, but I'm a cheapskate and didn't want to order extras, so I came up with this solution:
I cut all of the striking colors in half lengthwise and fired one half of each one. (I made a numbered map of the layout on the kiln shelf so I wouldn't mix any of them up)
Then I taped the halves back together (thought about copper foiling them, but I'm just as lazy as I am cheap)and stuck them back in the set. Done and done.
 
			
			
									
						
										
						I cut all of the striking colors in half lengthwise and fired one half of each one. (I made a numbered map of the layout on the kiln shelf so I wouldn't mix any of them up)
Then I taped the halves back together (thought about copper foiling them, but I'm just as lazy as I am cheap)and stuck them back in the set. Done and done.

- 
				gone
Have you seen pimento? I has "Jackie" written all over it.Jackie Beckman wrote:They have lots of special colors that aren't considered stock. But they only have them sometimes, so don't get spoiled with one! Spicy Orange is not really Terra Cotta colored. I happen to love the color, so if you know my pallette, that should give you some idea of what it's like. Tomato too. Yum!Special order colors !!! "Ooohhh, I asked, what else is available in special order?" Well, they have, in addition to the caramel, a Persimmon Red, Spicy Orange (hoping this is a terra cotta color), Tomato Red and deep red.
- 
				Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
Have you seen pimento? I has "Jackie" written all over it.
Ooohhh yes. If you look in the gallery here Els, the piece called Intrigue In Red is Tomato and Pimento together. It's my favorite pairing and when I start a new piece I have to force myself not to use it every time!
 All reds are good reds, but these are the best reds.
 All reds are good reds, but these are the best reds.