I moved. Ive lost my firing log. My life may be over.
anyways, now I need a recipe for plater water for 1500 deg casting. I need a volume one not weight. Does anyone have one? thanks if you can help.
Liam
plaster water ratio
Moderators: Brad Walker, Tony Smith
plaster water ratio
W.W.S.D.
(what would spab do)
(what would spab do)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: plaster water ratio
As much plaster mix as you can get in the water and still manage to get a pour with some resolution. The less plaster to water, the easier it is to pour and the weaker the mold. More plaster, stronger mold.Liam wrote:I moved. Ive lost my firing log. My life may be over.
anyways, now I need a recipe for plater water for 1500 deg casting. I need a volume one not weight. Does anyone have one? thanks if you can help.
Liam
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
charlie holden
- Posts: 260
- Joined: Thu Mar 13, 2003 8:26 pm
- Location: Atlanta