Hi, all, here's a finicky question:

I have small pieces of glass, diamond-shaped, standing up vertically in the kiln. They are held by slots in a mold that comes up to half their height. So half of their height is standing up vertically without anything to lean on. I want it this way so I can nicely fire polish the edges and both sides of the part that's standing free. The problem is, at fire polishing temperature the glass starts to slump over.

I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?

Thanks,
David
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Getting a fire polish without slumping

Post by Brad Walker »

dblood wrote:I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?
Nope.

Fire polishing takes place at a higher temperature than slumping, so it will slump before it fire polishes. The type of kiln or rate of temperature increase doesn't matter.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Getting a fire polish without slumping

Post by Bert Weiss »

dblood wrote:Hi, all, here's a finicky question:

I have small pieces of glass, diamond-shaped, standing up vertically in the kiln. They are held by slots in a mold that comes up to half their height. So half of their height is standing up vertically without anything to lean on. I want it this way so I can nicely fire polish the edges and both sides of the part that's standing free. The problem is, at fire polishing temperature the glass starts to slump over.

I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?

Thanks,
David
You can grind and polish by hand, not an easy job. 120 grit, 200 grit, 400 grit, cork belt, cerium oxide and felt wheel...
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
dblood
Posts: 24
Joined: Sat Jan 17, 2004 9:59 am
Location: Nashua, NH

Post by dblood »

Thank you for the replies. I guess I will see if I can finagle the fire polish before the tips slump too much. A little bit of slumping over might be nice actually...