Hi, all, here's a finicky question:
I have small pieces of glass, diamond-shaped, standing up vertically in the kiln. They are held by slots in a mold that comes up to half their height. So half of their height is standing up vertically without anything to lean on. I want it this way so I can nicely fire polish the edges and both sides of the part that's standing free. The problem is, at fire polishing temperature the glass starts to slump over.
I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?
Thanks,
David
Getting a fire polish without slumping
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Getting a fire polish without slumping
Nope.dblood wrote:I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?
Fire polishing takes place at a higher temperature than slumping, so it will slump before it fire polishes. The type of kiln or rate of temperature increase doesn't matter.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Getting a fire polish without slumping
You can grind and polish by hand, not an easy job. 120 grit, 200 grit, 400 grit, cork belt, cerium oxide and felt wheel...dblood wrote:Hi, all, here's a finicky question:
I have small pieces of glass, diamond-shaped, standing up vertically in the kiln. They are held by slots in a mold that comes up to half their height. So half of their height is standing up vertically without anything to lean on. I want it this way so I can nicely fire polish the edges and both sides of the part that's standing free. The problem is, at fire polishing temperature the glass starts to slump over.
I'm using a Paragon Quickfire kiln, which heats up VERY fast. Could I get the fire polishing without slumping if I heated up slower?
Thanks,
David
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions