Hi All,
I have made a few wall pockets and I have been using the inch-thick Ceramaguard fibre board sold on this site to form the pocket. After fusing, I have to soak in water and dig the fiber board out. It's pretty tough to get it all out.
My question is, is there something else I could use so that it will slide out from between the glass after firing and then I could re-use it? What if I coated the Ceramaguard with kiln wash?
Thanks for any suggestions.
Joy
Wall pocket seperator Q
Moderators: Brad Walker, Tony Smith
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
What about 1/8th thick fiber paper stacked to the depth you want? I use that for kiln carving, underneath my glass, and it releases pretty cleanly.
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
-
Joy
-
Cynthia
You can get fiber paper in 1/8 and 1/4 thicknesses. I would think you will want something a little thicker than Thinfire to give you the buffer you want to allow you to pull out your form.Joy wrote:Something like Thinfire? Or is there some other kind of flexable fibre paper?or the ceramaguard wrapped in fiber paper
Thanks!
Joy
-
Cynthia
You can get fiber paper in 1/8 and 1/4 thicknesses. I would think you will want something a little thicker than Thinfire to give you the buffer you want to allow you to pull out your form.Joy wrote:Something like Thinfire? Or is there some other kind of flexable fibre paper?or the ceramaguard wrapped in fiber paper
Thanks!
Joy
-
Joy