I just ordered dome stuff from Thompson Enamels & I noticed they had various sizes of 'Marinite Board' for sale.
I am not familiar with this & was wondering, is it useful in fusing, say for slumping molds or as a kiln shelf?
Marinite Board
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Marinite Board
I'm surprised to hear that Thompson would be selling Marinite. It warps pretty badly at the temps we work at.quill wrote:I just ordered dome stuff from Thompson Enamels & I noticed they had various sizes of 'Marinite Board' for sale.
I am not familiar with this & was wondering, is it useful in fusing, say for slumping molds or as a kiln shelf?
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Thompson enamels mature around 1400ºF which is similar to fusing. I wouldn't spend my money on another marinite board.quill wrote:It was advertised for use with enamels not fusing, I just wondered if it would work with fusing.It warps pretty badly at the temps we work at.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Jacques Bordeleau
I tried it for a 24x55 kiln shelf years ago. It warped like a pototo chip, blistered, and cracked .... not all on the first firing. Pretty much sucks for anything above low-fire enamels 1100-1200 degrees. The factory couldn't believe it, since it is rated much higher (2,000?) and did replace the 4x8' sheet....which also failed. I still have one more piece leftover. I'm waiting for someone really smart to tell me how to use it without these problems....hahahahah. Save your money.
regards, Jacques
regards, Jacques