Glass stuck on the kiln shelf
Moderators: Brad Walker, Tony Smith
-
Nancy Juhasz
- Posts: 113
- Joined: Sun Mar 09, 2003 10:10 pm
- Location: Ohio
Glass stuck on the kiln shelf
Well here I am again with a real mess. I tried slumping two bottles on the same shelf. I measured to make sure there was room for them to flatten before I closed the kiln very carefully. I opened it to flash vent when I found the mess. One of the bottles had flattened and run over the edge of the shelf.
It is to hot to get into the kiln yet plus I want to save the other bottle and the stuff I have on the shelf below. Don't know if the stuff (more bottles) on the bottom shelf is ruined or not since I can't see. How on earth do I get the melted glass off my shelf. It was well washed but I never wash the edges. I will in the future. Can I chip away at this glass and maybe grind it on my grinder or will I damage the shelf? Will it hurt to leave a little glass on the edge of the shelf. As you can see I have no idea what to do. This is the first disaster with my kiln. Thanks for any suggestions you have after you get done laughing at the new kid.
Nanc
-
Allan Gott
- Posts: 19
- Joined: Mon Mar 10, 2003 11:57 am
- Location: Calgary
- Contact:
Don't panic kiddo....all is not lost, hope the bottom shelf holds a pleasant suprise. Yes you can use your grinder on the shelf edge to clean off anything that stuck, use lots of water and go slow.
Think of it as a demonstration of how much hotter it is at the top of your kiln.
Allan
(been there done that hot glassmaker)
Think of it as a demonstration of how much hotter it is at the top of your kiln.
Allan
(been there done that hot glassmaker)
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact: