Fuse compatible glass when casting?

Post by coolntn »

Must I use fusing compatbile glass when doing a casting of a single color and from the same sheet of glass ?

If I'm mixing multiple glass I understand the necessisity to ensure all glasses are compatible. But what about a single color, from same sheet ?

Thanks a ton,
Still a casting newbie.
Russell simms
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Virtually all sheets are compatible with themselves, so if you're using only sheet, you shouldn't have to worry about compatibility.