Need to find silicon carbide flat lap pads
Moderator: Brad Walker
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact:
Need to find silicon carbide flat lap pads
I have a chance to purchase some polishing and grinding pads from another glass artist. I need to find silicon carbide flat lap pads, so I can figure out what a fair price would be for them. Any ideas? I can find diamond disks, but not the others.
Thanks
Steph
Thanks
Steph
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Need to find silicon carbide flat lap pads
I cant realy C any advantage of silicon carbide flat lap padsSteph Mader wrote:I have a chance to purchase some polishing and grinding pads from another glass artist. I need to find silicon carbide flat lap pads, so I can figure out what a fair price would be for them. Any ideas? I can find diamond disks, but not the others.
Thanks
Steph
U mean on a flat bed type thing
They wont last long loose grit is probably better

-
Jack Bowman
- Posts: 127
- Joined: Mon Mar 17, 2003 10:52 pm
- Location: Utah
- Contact:
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact:
Thanks, that price reference gives me some idea at least. I had a flat lap grinder made, and I bought an 80 grit diamond pad. For as little as I grind, I thought I could try these for a while, and there is a cork & prepolish pad as well that I can use. I hate to offer a price when I have no idea at all what they are worth. What industry would use these, anyway? I need to find a price reference somewhere.
-
Jack Bowman
- Posts: 127
- Joined: Mon Mar 17, 2003 10:52 pm
- Location: Utah
- Contact:
You might check with a rock shop. I've just never heard of a SiC pad if it's metal like the diamond ones. Not cost effective. I've worked with laps for many years as a machinist but the abrasives, whatever they were, were fed onto a cast iron plate. This thing you are talking about sounds like a SiC sanding disc to me. Maybe you could ask the owner where he got it. I'm relativly new to machining glass but I'm not impressed with SiC as compared to diamond. I feel the extra cost is worth it. You might go over to the kiln forming board and ask the same question as there are quite a few with much experience lapping glass.
Jack
Jack
HI,
I've been a lapidary longer than a glass worker..
Silicon Carbide is a fine choice for glass...
I use both Diamond and SC.. Diamond for all the rock work I do.
The expense is not necessary for occasional glass grinding.
Diamond, requires more water, but is cleaner. SC grinding tends to need a little more clean up.
SC will be a fraction of the cost, another plus. Depending on the size of the lap, 10' 12' ? any where from $1.50 to $5.00. Diamond, hundreds.
Check out places like, Rio Grande, Indian Jewelers Supply, and go to the Lapidary Journal web site for a list of suppliers.
JC
I've been a lapidary longer than a glass worker..
Silicon Carbide is a fine choice for glass...
I use both Diamond and SC.. Diamond for all the rock work I do.
The expense is not necessary for occasional glass grinding.
Diamond, requires more water, but is cleaner. SC grinding tends to need a little more clean up.
SC will be a fraction of the cost, another plus. Depending on the size of the lap, 10' 12' ? any where from $1.50 to $5.00. Diamond, hundreds.
Check out places like, Rio Grande, Indian Jewelers Supply, and go to the Lapidary Journal web site for a list of suppliers.
JC
"Without art we are merely monkeys with car keys" Joe Grant
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact:
HI,
I did a little checking and I still haven't found anyone with 24" discs.. most of the units being produced now are free abrasive types..
You can find the Lapidary Journal at;
http://www.lapidaryjournal.com
I didn't see anyone in the resource center w/ them that big either.
I'll do some looking today and see what I can find.
Warmly,
JC
I did a little checking and I still haven't found anyone with 24" discs.. most of the units being produced now are free abrasive types..
You can find the Lapidary Journal at;
http://www.lapidaryjournal.com
I didn't see anyone in the resource center w/ them that big either.
I'll do some looking today and see what I can find.
Warmly,
JC
"Without art we are merely monkeys with car keys" Joe Grant
http://www.mscdirect.com/IWCatProductPa ... &Keyword=Y
Haven't found any SC, this will give you an idea of the price and would work on glass.
JC
Haven't found any SC, this will give you an idea of the price and would work on glass.
JC
"Without art we are merely monkeys with car keys" Joe Grant
-
Steph Mader
- Posts: 59
- Joined: Tue Mar 11, 2003 1:45 am
- Location: Freeland, WA
- Contact: