This piece was made by Robin Mix. Can anyone tell me what does MURINI means? Her work is great and I think done as a roll up.
http://www.sandraainsleygallery.com/fra ... rtistID=25
Thanks,
BobB
Green Murini vase
Moderators: Brad Walker, Tony Smith
Re: Green Murini vase
think of a pattern bar. a hunk of glass built up of other rods, slabs, etc. fuse into a bar. and instead of being saw cut into slices, is heated and pulled into a BIG stringer. then take slices off that.BobB wrote:This piece was made by Robin Mix. Can anyone tell me what does MURINI means? Her work is great and I think done as a roll up.
http://www.sandraainsleygallery.com/fra ... rtistID=25
Thanks,
BobB
-
Melissa Terman
- Posts: 52
- Joined: Tue Mar 18, 2003 1:07 am
- Location: New York
- Contact:
la murrina (singular), le murrine (plural)
Cross-sectional pieces of cane. An age-old Venetian technique by which bundles of cane (rod) are assembled, heated and stretched so as to create specific imagery within the resulting cane.
I lifted the definition from, "Advanced Glassworking Techniques" Edward T. Schmid
What can be done with murrine is incredible. Check out the work of Dinah Hulet. She makes portraits in murrine http://www.dinahhulet.com
Cross-sectional pieces of cane. An age-old Venetian technique by which bundles of cane (rod) are assembled, heated and stretched so as to create specific imagery within the resulting cane.
I lifted the definition from, "Advanced Glassworking Techniques" Edward T. Schmid
What can be done with murrine is incredible. Check out the work of Dinah Hulet. She makes portraits in murrine http://www.dinahhulet.com