:!: I want to thank all who have helped me get this slumping thing going I have just made some serving dishes with the glass from my mother-in'laws home and also some from some glue chip that I sell in my stained glass store, now I would like to put some color on them where can I get some colored frit that will work with this float glass without having to buy it by the pound, I hope to hear from someone on this I know I an also paint color on but the frit would look great.
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

CR loo sells frit for float glass. You must test it for compatibility to make sure it will work with your glass.

http://crloo.com/Products/Float_Glass/float_glass.html


Paradise Paints sells glass paints that seem to work with just about any glass.

http://www.paradise-co.com/paints/
Judy Schnabel
Posts: 195
Joined: Mon Mar 10, 2003 9:45 pm
Location: SW FL
Contact:

Post by Judy Schnabel »

You can also get confetti & powders that are float-compatible from CR Loo.