lettering on food-friendly glass

Post by Bonnie Rubinstein »

Helllo happy fusers.. I am new to this- can anyone recommend a safe way to paint letters on a plate that will hold food. The gold paint I have has lead.. should I buy other paints ( is there lead-free gold?), or place a clear piece over the my gold after it has been fused and fire again? Would this diffuse the quality of the lettering? Ideas? Thanks!
8)
Bonnie Rubinstein
Dick Ditore
Posts: 58
Joined: Mon Mar 10, 2003 12:56 pm
Location: San Diego, Ca
Contact:

Post by Dick Ditore »

paint it on, fire it, and clear cap it.

Dick
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Post by Bonnie Rubinstein »

Dick, won't this diffuse the sharpness of the lettering?