http://www.etchworld.com - sand etch sandblaster...
it's tiny and it's cheap so it _sounds_ ideal, but does anyone have any experience with this thing? i just need to sandblast really small things, 4x4" max....will this do?
also, as a possible alternative i was looking into etch bath dipping solutiob, but i was hoping to be able to fire my pieces after i etch/sandblast them to get that satiny look...would that work if it was a chemical etch?
thanksssss
peace
- l
etchworld sand etch...
Moderators: Brad Walker, Tony Smith
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
It will work, but you'll outgrow it quickly and you'll want more.
With that said, try to minimize the amount of grit that gets all over the place by blasting in a cardboard box or storage tub. The clear tubs work better than the opaque tubs since they let light through.
Compared to setting up a sandblaster and cabinet, it's a small investment, so you should go for it. I don't know how long the cans of air will last... I can't imagine you'll get too many pieces out of a can, but I would be curious to know what you learn.
Tony
With that said, try to minimize the amount of grit that gets all over the place by blasting in a cardboard box or storage tub. The clear tubs work better than the opaque tubs since they let light through.
Compared to setting up a sandblaster and cabinet, it's a small investment, so you should go for it. I don't know how long the cans of air will last... I can't imagine you'll get too many pieces out of a can, but I would be curious to know what you learn.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Dale Grundon
- Posts: 5
- Joined: Sun Mar 09, 2003 6:13 pm
- Location: Mt. Gretna PA
- Contact: