The pot melts are also terracotta and are not kiln-washed and don't stick, thus the question.  I also fire in clay molds, albeit shallow, that are not kiln-washed and my glass doesn't stick.  Of course, this is at low slumping temps.  However, the pot melts are quite hot.  Yet, the glass still doesn't stick.  Or maybe there is some residual glass in the pot... can you pot melters tell us?  Thanks.
Ms. Trying-to-avoid-more-kilnwash
			
			
									
						
										
						Ms. Trying-to-avoid-more-kilnwash
- 
				Ron Coleman
 - Posts: 468
 - Joined: Sun Mar 09, 2003 3:20 pm
 - Location: Columbus, Ohio USA
 
The pot melts do leave a layer glass in the pots. After cooling they ping and pop for a long time as the glass shrinks and cracks. I have 2 sitting on the bench that are about 2 weeks old and still ping once in a while.Dani wrote:The pot melts are also terracotta and are not kiln-washed and don't stick, thus the question. I also fire in clay molds, albeit shallow, that are not kiln-washed and my glass doesn't stick. Of course, this is at low slumping temps. However, the pot melts are quite hot. Yet, the glass still doesn't stick. Or maybe there is some residual glass in the pot... can you pot melters tell us? Thanks.
Ms. Trying-to-avoid-more-kilnwash
The pings give you a good scare while you're working on other glass.
I think if you wash the pots it will mix with the glass as it slides down and out.
Ron
- 
				tattooedpanda
 - Posts: 8
 - Joined: Wed Mar 19, 2003 9:53 pm
 
what to do with your scrap
there are many of us small guys that wouls love to be able to get some of this scrap to make our jewlery  
  I cannot afford to buy some of each color and I try to buy bullseye scrap when I can find it. I teach a small jewery fusing class and the small stuff works great for pins and earrings. I would say you would have no problem selling it by the pound in random mixed lots though here or on ebay you can ship up to 3 pounds anywhere in the use for $3.85 in a flat rate envelope I do it all the time with my regular stained glass I sell as mosiac tumble glass.  
 please let me know  Andy